        common problem

        Under what conditions can spray welding be used?

        author:admintime:2019-09-22 22:20click:
                    Spray welding is to reheat the preheated self-soluble alloy powder coating to 1000-1300 C, melt the particles, float the slag onto the surface of the coating, and disperse the boride and silicide in the coating, so as to achieve good bonding between the particles and the surface of the substrate.
                    Spray welding process is suitable for the following situations:
                    1. Surface loads of various kinds of carbon and low alloy steels are large, especially those subjected to impact loads. For workpieces with bonding strength of 350-450N/mm2, spray welding hardness HRC150 < 65, coating thickness from 0.3 to several millimetres, and surface roughness of spray welding layer after grinding can reach Ra0.4-0.1 micrometres.
                    2. When used in corrosive media, the coating is required to be compact and porous.
                    3. Hardening, carburizing, nitriding and hard chromium plating are used in the original design of workpiece surface, which requires high hardness.
                    4. Workpiece working environment is bad, such as strong abrasive wear, erosion wear, cavitation and so on.
                    5. Oxygen-acetylene flame alloy powder spray welding process is suitable for surface strengthening or repairing of various carbon steel and low alloy steel parts, but some characteristics of parts material should be noticed. When the linear expansion coefficient of matrix material differs greatly from that of alloy spray welding layer, it should be used cautiously when the linear expansion coefficient of matrix material is less than 12 *10-6/~C and more than 12 *10-6/~C, so as to avoid manufacturing. Cracks can also be difficult to spray welding if the content of elements with high affinity to oxygen in matrix metals is more than 3%, the total content of elements such as tungsten and molybdenum is more than 0.5%, or the sulfur content in steel is more than 0.5%. This is because these materials are easy to form dense and stable oxide film by interaction with oxygen to prevent melting. The wetting effect of the alloy on the matrix will cause the liquid alloy to roll like a "sweat bead" during remelting. Therefore, the adaptability of the spray welding process to the sprayed matrix material should be paid attention to.
                    6. Metal materials that can be sprayed without special treatment:
                    7. Metal materials that need to be preheated at 250-375 C after spray welding need to be slowly cooled.
                    8. Metal materials requiring isothermal annealing after spray welding

        Telephone

        0769-85415700

        function

        Price

        quality

        service

        Wechat sweep

        Mobile phone sweep

        主站蜘蛛池模板: 蜜臀av在线播放| 26uuu在线欧美| 蜜桃?一区二区视频在线观看| 午夜激情网站| 欧韩一区| 亚洲欧洲日韩综合色天使不卡| av中文天堂| 无码h片| 日本色色网| 茌平县| 欧美日韩另类在线| 91高清国产| 91露脸熟女对白不带套| 文山县| 欧美a√| 日韩在线观看a| 十八禁黄网站| 久草国产手机视频在线观看| 日韩AV第一页在线播放| 日韩a欧美| 亚洲黄色一区二区三区| 亚洲老熟女| 日本三级电影网| 免费国产va在线视频| 亚洲网在线| 亚洲中文字幕日韩| 男人天堂国产| 深夜免费福利| 遵义县| 久久精品99久久久久久久久| 婷婷伊人精品| 在线亚洲国模九九| 国产乱人伦| 午夜激情网站| 91高清在线观看| 国产精品美女久久久久久2021| 精品国产一区二区三区AV性色| 国产熟女在线播放| 2019亚洲男人天堂| 人人爽人人澡人人高潮| 九九热这里只有国产精品|